forumolz.blogg.se

Ironman mark 40 pepakura files
Ironman mark 40 pepakura files










Start applying one strip of Fiberglass Mat, and resin over it in the inner side of the part. Once the catalyst is added, you will only have 15 minutes to work with it aprox. As long as you work with this you will know how many drops you'll need). Mix a small portion of the resin (I used 1/4 of a cup) with the catalyst (10 to 20 drops, depending on the weather, if it's hot, with 10 drops it's ok. Put your gloves, protective eye glasses and respirator. Cut the Fiber Glass mat in small or big strips depending on the part size.

ironman mark 40 pepakura files

This will help us to avoid the resin stick to the table.

ironman mark 40 pepakura files

Second list of material: Fiber glass resin (with its hardener) Fiber glass mat Scissors Aluminium foil Aerosol Can Lubricant (WD-40) Gloves Paint Brushes Respirator Protective Eye Glasses Dremel Tool Prapare a table with Aluminium foil, spray lubricant over it.












Ironman mark 40 pepakura files